Peeled and ground round bars
Peeling turns the outer skin off a hot rolled round bar, taking the mill scale, surface seams and decarburised layer with it. Grinding then brings the bar to a precise size and a fine finish.
Peeled and ground bars are round steel bars whose outer layer has been turned off rather than compressed in, then centreless ground to size. Akansha Ispat supplies them for large and critical shafts and induction hardened parts, checked by magnetic particle and ultrasonic inspection, with a Mill Test Certificate.
| Size range | On request, typically above 20 mm |
|---|---|
| Process | Peeled, ground, straightened, polished |
| Typical tolerance class | h9 ground, h10 turned and peeled |
| Grades | All six quality groups, subject to size. See grades |
| Finish | Bright, fine ground surface |
| Typical uses | Large and critical shafts, induction hardened parts |
| Inspection | Magnetic particle and ultrasonic testing in house |
| Documents | Mill Test Certificate with every product |
Removed, not compressed
This is the whole argument for peeling, and it is worth being precise about. A hot rolled bar leaves the mill with a surface layer that is not the same steel as its core. It carries scale, it can carry rolled-in seams, and its outermost skin has lost carbon to the furnace atmosphere, which is called decarburisation.
What cold drawing does to that layer
Drawing pulls the bar through a die. The surface is burnished bright and the bar comes out to size, but the defective layer is still there. It has been compressed and smoothed, not taken away. For most parts this is entirely fine.
What peeling does instead
Peeling cuts the layer off as swarf. What is left is sound sub-surface metal with full carbon content. That matters when the part will be induction hardened, because a decarburised skin will not take hardness, or when the part is fatigue loaded and a surface seam would be a crack starter.
The trade-off is cost and yield: you are paying to turn good steel into swarf. Read the full comparison of cold drawn and peeled bars.
Four cases that justify the cost
- The part will be induction hardened. A decarburised surface will not reach the specified case hardness, and the problem is invisible until the part is tested.
- The bar is large. Above roughly 50 mm, drawing becomes difficult and peeling is the practical route to a bright bar.
- The surface is the working surface. Hydraulic rods, sliding shafts and sealing diameters, where a seam becomes a leak path.
- The part is fatigue loaded. Rotating shafts fail from the surface inward, so surface integrity is the design limit.
How we check them
Peeled and ground bars go through the same in-house inspection as the rest of our output, plus two checks aimed at exactly the defects peeling exists to remove.
- Magnetic particle inspection. Finds surface and near-surface cracks and seams.
- Ultrasonic testing. Finds internal defects such as inclusions and centre porosity.
- Mill Test Certificate. Chemical composition and mechanical properties for the heat supplied.
Peeled and ground round bars: common questions
What is a peeled bar?
A peeled bar is a round steel bar whose outer layer has been turned off on a peeling machine, removing mill scale, surface seams and the decarburised skin, rather than compressing them in as cold drawing does.
What is the difference between peeled and ground bars?
Peeling removes the outer layer. Grinding is a later operation that brings the bar to a precise diameter and a fine surface finish. A bar can be peeled only, or peeled and then ground.
Why does decarburisation matter?
A decarburised surface has lost carbon and will not reach the specified hardness when induction hardened. If the part relies on a hard case, the skin has to come off first.
What tolerance do peeled and ground bars hold?
Ground products are commonly supplied to ISO 286 class h9 and turned or peeled bars to h10. Confirm the class for your size and grade on the enquiry.
Are peeled and ground bars tested?
Yes. They are checked in house with magnetic particle inspection for surface defects and ultrasonic testing for internal defects, and supplied with a Mill Test Certificate.
Tell us the grade, size and quantity.
Send your requirement and our team will reply with availability and a quotation. Share a drawing if you have one.